One Product. Total
Microtrench Reinstatement.

Bonds to asphalt and concrete. Seals the trench. Protects everything beneath it.

Why Choose Us

Advanced Microtrench Sealant

Contractors cut 15 inches deep through city streets. Most fill it with plain concrete — it doesn’t bond, doesn’t seal, and eventually fails. Ultimate Street Armor is the top 3-inch layer cities can require. It bonds to both sides and seals the trench for good.

Bonds permanently to asphalt and concrete

Watertight seal — no intrusion, no subsurface swelling

Traffic-ready in 4 hours

Resistant to oils, fuels, and hydrocarbons

Near-zero shrinkage for a crack-free surface

The Proof Is in the Pavement

This Is What Wrong Looks Like — And What Right Looks Like

The gap between these two isn’t just cosmetic. It’s the difference between a street that lasts and one that fails. Cities can see the difference from the street. Now they can require the standard that makes it permanent.

Without Ultimate Street Armor

Unbonded fill. Open gaps. Water gets in — and the damage starts immediately.

With Ultimate Street Armor

Clean seal. Bonded to both surfaces. No gaps, no water, no early failure.

Technical Data

The Numbers Behind the Performance

All values tested at 75°F (24°C) per ASTM standards.

Property
Value
Water Demand
~3 quarts/bag
Working Time
20 minutes
Compressive Strength (ASTM C109) — 4 Hour
2,225 psi
Compressive Strength (ASTM C109) — 1 Day
3,175 psi
Compressive Strength (ASTM C109) — 7 Day
5,575 psi
Compressive Strength (ASTM C109) — 28 Day
6,125 psi
Tensile Strength (ASTM C190) — 7 Day
435 psi
Tensile Strength (ASTM C190) — 28 Day
585 psi
Flexural Strength (ASTM C348) — 7 Day
845 psi
Flexural Strength (ASTM C348) — 28 Day
1,400 psi
Adhesion (ACI 503.R)
>290 psi
Bond Strength (ASTM C882) — 1 Day
Bond Strength (ASTM C882) — 7 Day
Water Absorption (ANSI A118.7)
<4.0%
Length Change (ASTM C157)
< 0.04%
Initial Set (ASTM C191)
31 min.
Final Set (ASTM C191)
39 min.
Rapid Chloride Permeability (ASTM C1202)
Modulus (ASTM C469)
Thermal Expansion (AASHTO T366)

Tested to Standards That Matter

ASTM C109

Compressive strength from 4 hours to 28 days

ASTM C190

Superior tensile resistance against cracking

ASTM C348

High flexural strength with microfiber reinforcement

ASTM C157

Extremely low shrinkage under 0.04%

ASTM C191

Rapid and precise set times

ASTM C882

Tenacious bond strength exceeding industry standards

ASTM C1202

High durability with low chloride ion penetration

AASHTO T-336

Low thermal expansion for extreme conditions

Scroll to Top